Industrial imaging and materials analysis for foundry and metallurgy

X-ray tomography, metallography, SEM-EDX and hardness measurements: INSIDIX inspects your cast, forged and sintered parts without destroying them, in Grenoble.

  • 30 years of expertise in industrial imaging
  • 320 kV for dense metallic parts
  • 5 gf to 10 kgf of automated Vickers hardness

Foundry & metallurgy sector

Non-destructive testing of cast, forged and sintered parts

In foundry and metallurgy, internal defects — shrinkage porosity, blowholes, inclusions, cracks — can lead to failures in service. They escape visual inspection. INSIDIX inspects your cast, forged or sintered parts without destroying them, to guarantee their structural integrity.

Our Grenoble laboratory combines X-ray tomography (up to 320 kV for dense metallic parts), 3D metrology and materials analysis: metallographic cross-sections, SEM-EDX and hardness measurements. We locate and measure defects, then trace them back to their cause, which speeds up validation and reduces scrap.

To understand the origin of a failure, also discover our forensic expertise and failure analysis.

Your challenges

Recurring issues

  • Shrinkage porosity and blowholes Cast parts, foundry.
  • X-ray tomography of cast parts Foreign bodies in alloys
  • Internal cracks Cast, forged, sintered
  • Welds and brazed joints Metallic assemblies
  • Dimensional inspection Complex internal geometry
  • Fracture, microstructure and hardness Fracture surfaces, cross-sections and Vickers measurements.

Support

From scoping to report

Scoping the analysis Choice of technique with you according to the alloy, the part size and the defect sought.
Inspection and analysis X-ray tomography to locate defects, then metallographic cross-section, SEM-EDX or hardness measurement to find their cause.
Deliverables Report, annotated images, 2D and 3D views and measurement data, usable for qualification or failure analysis.

Case · X-ray radiography of a foundry part

Feasibility of radiographic inspection on a large aluminium part

A customer entrusts us with a large cast aluminium alloy part (approximately 43 × 28 × 7 cm, three thickness zones). Objective: find out whether X-ray radiography can inspect it and identify foundry defects. Five views are taken, with an image quality indicator suited to each thickness.

Porosités : flèches jaunes (vue 1)

Porosity

yellow arrows (view 1)
Retassure : zone cerclée (vue 2)

Shrinkage

circled area (view 2)
Microporosités : zone épaisse (vue 6)

Microporosity

thick area (view 6)
Method X-ray radiography in five views, with an image quality indicator (IQI, visible on the images) per thickness range, detectability of 60 to 80 µm.
What you see Porosity, shrinkage and a microporosity zone, marked on each view by arrows and ovals.
Reference standard The indications are then classified by comparison with ASTM E155 reference radiographs, the standard for aluminium and magnesium castings.
Deliverable Report with annotated views and recorded indications, ready for the final diagnosis.

Case · X-ray radiography and tomography

Compliant or non-compliant part: where are the lower-density zones?

Two foundry samples, one judged compliant (OK) and the other non-compliant (NOK), are compared by radiography (40 µm resolution) then by tomography (70 to 75 µm). Objective: locate cracks, shrinkage and lower-density zones, and see what distinguishes the two parts.

Échantillon 1 (NOK) : radiographie

Sample 1 (NOK)

radiography
Échantillon 3 (OK) : radiographie

Sample 3 (OK)

radiography
Échantillon 3 · tomographie : coupe 2D, défauts localisés

Sample 3 · tomography

2D slice, defects located
What you see Cracks or shrinkage (red) and lower-density zones (yellow) on both samples, more on the OK sample.
Deliverables Video and 2D images of each sample, 3D view and 2D slices of the OK sample.

Case studies

Our case studies

Real analyses carried out in the laboratory, presented anonymously: the problem, the method and the results.

INSIDIX

Why choose INSIDIX for your metal parts?

  • Icône inspection — valeur INSIDIX 30 years of expertise Industrial imaging and non-destructive testing
  • Icône composition et biocompatibilité — valeur INSIDIX Several techniques A single laboratory to locate and then understand
  • Icône inspection — valeur INSIDIX Usable report Annotated images, measurements and 3D views
  • Icône composition et biocompatibilité — valeur INSIDIX Confidentiality Your parts and results remain protected

FAQ

Frequently asked questions about inspecting metal parts

X-ray tomography reveals shrinkage porosity, blowholes, inclusions and internal cracks, without cutting the part.

Yes. Our Nikon XT H 320 tomograph has a 320 kV source suited to dense parts. Feasibility depends on the alloy and the size of the part: we assess it with you.

We locate the defect by tomography, then observe it under the SEM with EDX analysis of the local composition, possibly after a metallographic cross-section.

Yes, with the laboratory’s automatic hardness tester, in Vickers and micro-Vickers hardness from 5 gf to 10 kgf.

Yes. X-ray tomography inspects the inside of welds and brazed joints, and a metallographic cross-section makes it possible to examine their structure.

Contact us describing your part, its alloy and the defect sought. We define the analysis plan with you, while respecting the confidentiality of your projects.

Have your metal parts inspected.

Describe your part, its alloy and the defect sought: we will propose the appropriate analysis plan.